Na voljo sta dva načina iskanja: enostavno in napredno. Enostavno iskanje lahko zajema niz več besed iz naslova, povzetka, ključnih besed, celotnega besedila in avtorja, zaenkrat pa ne omogoča uporabe operatorjev iskanja. Napredno iskanje omogoča omejevanje števila rezultatov iskanja z vnosom iskalnih pojmov različnih kategorij v iskalna okna in uporabo logičnih operatorjev (IN, ALI ter IN NE). V rezultatih iskanja se izpišejo krajši zapisi podatkov o gradivu, ki vsebujejo različne povezave, ki omogočajo vpogled v podroben opis gradiva (povezava iz naslova) ali sprožijo novo iskanje (po avtorjih ali ključnih besedah).

Pomoč
Išči po:
Možnosti:
 


1971 - 1980 / 2000
Na začetekNa prejšnjo stran191192193194195196197198199200Na naslednjo stranNa konec
1971.
The corrosion properties of steel in pore solutions obtained from alkali‐activated mortars
Nina Gartner, Tadeja Kosec, Stéphane Poyet, Andraž Legat, 2023, izvirni znanstveni članek

Povzetek: Alkali‐activated materials (AAMs) are considered a promising alternative to materials made from ordinary Portland cement (OPC). Other than considering the durability of the material itself, the use of AAMs for reinforced concrete elements also raises the question of steel corrosion processes in these materials, which are still relatively unknown. Three different alkali‐activated mortars were prepared for this study, based on either fly ash, slag, or metakaolin. Pore solutions were then extracted from each mortar and chemically analyzed. Electrochemical techniques were used to study the corrosion of steel in synthetic pore solutions containing varying concentrations of chlorides. In parallel, the same corrosion tests were performed in a generic pore solution representing OPC mortar. It was shown that the chemical composition differed in each pore solution tested, thus affecting the corrosion properties of the steel. The addition of chloride also had a varying effect on the corrosion properties of the steel in each type of pore solution tested. This study provided a basic overview of the corrosion behavior and mechanisms of the various AAM environments in comparison to that of OPC.
Ključne besede: alkali-aktivated materials, corrosion, electrochemical corrosion techniques, extracted pore solution
Objavljeno v DiRROS: 20.11.2023; Ogledov: 369; Prenosov: 102
.pdf Celotno besedilo (2,73 MB)
Gradivo ima več datotek! Več...

1972.
Influence of structural parameters of nonwoven geotextiles on separation and filtration in road construction
Špela Bezgovšek, Dunja Šajn Gorjanc, Boštjan Pulko, Stanislav Lenart, 2020, izvirni znanstveni članek

Povzetek: Nonwoven geotextiles are often used in road construction as a separation layer. They consist of the web of fibers with different orientations. The orientation of fibers has an important influence on physical and mechanical properties of nonwoven geotextiles. The production of nonwoven geotextiles is cheaper in comparison to woven or knitted fabrics which can also be used as separation geotextiles. The purpose of this research was to study the influence of structural properties of nonwoven geotextiles, namely the diameter of fibers and mass and thickness of nonwoven geotextiles, on their mechanical and hydraulic properties. Six types of nonwoven geotextiles were used in the research. They were produced by the drylaid process (carded) using mechanical bonding technique and also with the combination of mechanical and thermal bonding technique. The research confirmed that the bonding technique and structural properties significantly influence the separation and filtration properties of nonwoven geotextiles, such as opening size and water permeability. It was also found that there are no significant differences in mechanical properties, such as viscoelastic properties and compression creep, between the samples in the dry and wet conditions.
Ključne besede: nonwoven geotextiles, bonding techniques, opening size, water permeability
Objavljeno v DiRROS: 16.11.2023; Ogledov: 523; Prenosov: 205
.pdf Celotno besedilo (1,74 MB)
Gradivo ima več datotek! Več...

1973.
Dynamic properties of lightweight foamed glass and their effect on railway vibration
Stanislav Lenart, Amir M. Kaynia, 2019, izvirni znanstveni članek

Povzetek: Deformation properties of lightweight coarse grained material from recycled foamed glass have been determined from large-scale triaxial tests on prismatic specimens with dimensions 40 cm x 40 cm x 80 cm. Deformations were measured locally using vertical and horizontal local deformation transducers. Monotonic and cyclic loading at small to medium strain range were conducted. Three load sequences representing the expected conditions of use of lightweight material as vibration-reducing material in railway geotechnics have been used. Results indicate strong effect of brittle cellular structure of tested material as well as confining pressure dependency of elastic threshold shear strain and damping ratio. The results were used to assess the applicability of empirical formulas for shear modulus of granular materials to lightweight foamed glass. The parameters determined from the laboratory tests were further used in numerical analysis of railway dynamic response. The results of the numerical simulations show that replacement of fill in track embankment by lightweight material could improve the dynamic response of the track in reducing the vibration.
Ključne besede: lightweight material, recycled foamed glass, railway vibration, shear modulus, damping
Objavljeno v DiRROS: 16.11.2023; Ogledov: 436; Prenosov: 300
.pdf Celotno besedilo (2,12 MB)
Gradivo ima več datotek! Več...

1974.
Corrosion properties of aluminized 16Mo3 steel
Blaž Karpe, Klara Prijatelj, Milan Bizjak, Tadeja Kosec, 2023, izvirni znanstveni članek

Povzetek: Chromium-molybdenum steel (16Mo3) is widely used in petroleum, gas, automotive, and construction industries due to its good oxidation resistance and mechanical properties at moderately elevated temperatures. The aim of the research was to evaluate the corrosion susceptibility of 16Mo3 steel in hot rolled and aluminized states. Aluminization was performed by diffusion pack aluminization process at 900°C/2h and 730°C/4h, respectively. Electrochemical corrosion testing included measuring open circuit potential (EOCP), linear polarization resistance (LPR), potentiodynamic polarization, and electrochemical impedance spectroscopy (EIS) in potassium phosphate buffer (KH2PO4, pH = 7). Optical microscopy (OM), scanning electron microscopy (SEM), and energy dispersive X-ray spectroscopy (EDS) were used for surface layer microstructure characterization before and after corrosion tests. It was demonstrated that corrosion resistance of aluminized steel increased substantially. Corrosion properties were related to the structure and properties of intermetallic phase (FeAl, FeAl2 and Fe2Al5) that formed on the surface of 16Mo3 steel.
Ključne besede: aluminide coatings, aluminized steel, aluminizing, electrochemical corrosion investigation, 16Mo3 steel
Objavljeno v DiRROS: 16.11.2023; Ogledov: 474; Prenosov: 249
.pdf Celotno besedilo (4,40 MB)
Gradivo ima več datotek! Več...

1975.
Accounting for cloud cover and circannual variation puts the effect of lunar phase on deer–vehicle collisions into perspective
Jacopo Cerri, Laura Stendardi, Elena Bužan, Boštjan Pokorny, 2023, izvirni znanstveni članek

Povzetek: Although several studies have focused on the influence of moonlight on deer–vehicle collisions, findings have been inconsistent. This may be due to neglect of the effects of cloud cover, a major impediment to moon illumination and circannual variation in both deer and human activity. We assessed how median cloud cover interacted with the illuminated fraction of the moon in affecting daily roe deer (Capreolus capreolus) roadkill in Slovenia (Central Europe). Data included nationwide roadkill (n = 49,259), collected between 2010 and 2019 by hunters, as required by law. Roadkill peaked under medium to high cloud cover and decreased during nights with low or extremely high cloudiness. This pattern was more pronounced on nights with a full moon. However, the effects of moon illumination and cloud cover had a lower predictive potential than circannual variation, as collisions clearly peaked in April/May, July and August/September. Our results suggest that moonlight could influence roe deer movements through compensatory foraging. However, on nights with a full moon, collisions could also be affected by weather. On bright nights, roe deer might be less active due to increased human presence and sustained vehicular traffic. Then, with medium to high cloud cover and also rainfall, human presence in the environment may be low enough to increase deer movements, but vehicular traffic can still be intermediate, maximizing the risk of collisions. Finally, with overcast skies, widespread rainfall can reduce both traffic volume and human outdoor activity, decreasing the risk of collisions. Moon illumination may indeed affect wildlife–vehicle collisions and roadkill, but its effects should be quantified as a function of cloud cover. Moreover, to make studies truly comparable, research about wildlife–vehicle collisions should also account for time of the year. Policy implications. Because collisions with roe deer peak at particular periods of the year, signs should be installed seasonally. By doing so, they would warn drivers about the risk, improve drivers' awareness and increase their safety. Moreover, as collisions also increase on nights with a full moon and overcast skies, interactive warning signs that are activated by ground illumination should also be useful.
Ključne besede: cloudiness, MODIS Surface Reflectance, moon, road ecology, roe deer, Slovenia, thin-plate splines, wildlife–vehicle collisions
Objavljeno v DiRROS: 16.11.2023; Ogledov: 541; Prenosov: 235
.pdf Celotno besedilo (4,25 MB)
Gradivo ima več datotek! Več...

1976.
Monitoring the galvanic corrosion of copper–steel coupling in bentonite slurry during the early oxic phase using coupled multielectrode arrays
Tadeja Kosec, Miha Hren, Klara Prijatelj, Bojan Zajec, Nina Gartner, Andraž Legat, 2023, izvirni znanstveni članek

Povzetek: In the case of a two-part container for spent nuclear fuel, consisting of an iron-based inner structure with a copper coating, the potential perforation of copper through minor damage may result in intensive galvanic corrosion between copper and steel. The present work focuses on the corrosion of steel galvanically coupled to copper and exposed to a slightly saline environment under oxic conditions. The electrochemical processes on individual electrodes were monitored by coupled multielectrode arrays (CMEAs). The CMEAs were either in contact with groundwater saturated with bentonite or immersed in groundwater only. Very high galvanic corrosion currents were detected between carbon steel and pure copper in the early oxic phase. Additionally, the use of CMEAs further made it possible to monitor the distribution of cathodic currents around the steel electrode, which behaved anodically. Various microscopy and spectroscopy techniques were applied to identify the modes of corrosion and the type of corrosion products present at the end of the period of exposure.
Ključne besede: copper, steel, bentonite, Aspö groundwater, coupled multi electrode array, electrochemical properties, Raman analysis, corrosion
Objavljeno v DiRROS: 16.11.2023; Ogledov: 560; Prenosov: 130
.pdf Celotno besedilo (1,66 MB)
Gradivo ima več datotek! Več...

1977.
Dobro je vedeti pred prvo (ali naslednjo) znanstveno objavo : Predavanje na Kolokviju GIS, 23. 10. 2023
Maja Peteh, 2023, druge monografije in druga zaključena dela

Ključne besede: odprta znanost, znanstvena komunikacija
Objavljeno v DiRROS: 16.11.2023; Ogledov: 549; Prenosov: 305
.pdf Celotno besedilo (3,77 MB)
Gradivo ima več datotek! Več...

1978.
1979.
1980.
Preface
Vasja Leban, Anže Japelj, Lidija Zadnik Stirn, Špela Pezdevšek Malovrh, 2023, predgovor, uvodnik, spremna beseda

Ključne besede: forest management, economics, conferences, preface
Objavljeno v DiRROS: 14.11.2023; Ogledov: 645; Prenosov: 193
.pdf Celotno besedilo (90,49 KB)